You have requested a machine translation of selected content from our databases. This functionality is provided solely for your convenience and is in no way intended to replace human translation. Neither SPIE nor the owners and publishers of the content make, and they explicitly disclaim, any express or implied representations or warranties of any kind, including, without limitation, representations and warranties as to the functionality of the translation feature or the accuracy or completeness of the translations.
Translations are not retained in our system. Your use of this feature and the translations is subject to all use restrictions contained in the Terms and Conditions of Use of the SPIE website.
18 December 2019Template-free sol–gel preparation of antireflection films with adjustable refractive index
A antireflection film with adjustable refractive index from 1.17 to 1.41 was prepared at room temperature via a template-free sol–gel method, using tetraethylorthosilicate(TEOS) as co-precursor. In this study, the regulation of the refractive index is achieved by mixing different volumes of acid-catalyzed silica sol having a refractive index of 1.41 with a base-catalyzed silica sol having a refractive index of 1.17. The silica coating, with a refractive index of 1.2332, prepared by this base/acid two step catalysis sol-gel process can increase the transmittance of K9 glass by about 3.5%.