You have requested a machine translation of selected content from our databases. This functionality is provided solely for your convenience and is in no way intended to replace human translation. Neither SPIE nor the owners and publishers of the content make, and they explicitly disclaim, any express or implied representations or warranties of any kind, including, without limitation, representations and warranties as to the functionality of the translation feature or the accuracy or completeness of the translations.
Translations are not retained in our system. Your use of this feature and the translations is subject to all use restrictions contained in the Terms and Conditions of Use of the SPIE website.
15 January 1996Strength degradation and recovery during zero-stress aging of fused silica optical fibers
The two-point bending technique has been used to measure the strength of both polymer coated and bare fibers in liquid nitrogen after the fibers were first aged in an aggressive environment followed by a drying process. The results show that some strength recovery occurs upon drying of polymer coated samples while continuing degradation was seen when drying bare samples. The healing process observed for coated fiber is thought to be caused by condensation of the hydrated surface layer formed during aging.
The alert did not successfully save. Please try again later.
Gilberto M. Camilo, M. John Matthewson, M. E. Menkes, "Strength degradation and recovery during zero-stress aging of fused silica optical fibers," Proc. SPIE 2611, Optical Network Engineering and Integrity, (15 January 1996); https://doi.org/10.1117/12.230122