We have developed a Cr-based attenuated phase shift mask process for 0.18 micrometer device generation. The fabrication process including formation of opaque patterns with an electric conductive material is introduced. With a Cr-based attenuated phase shifter material, it is possible to adjust phase angle using a post process of quartz etching after mask defect inspection. Phase and transmittance control satisfied requirements for attenuated phase shift masks (att-PSMs) of 0.18 micrometer generation. Preliminary investigation of printability for after repair of a small clear defect with a conventional focus ion beam (FIB) carbon deposition film is reported. A positive carbon deposition bias is effective to obtain a larger common ED-window, and a more feasible ED- window can be obtained with a thinner carbon deposition film. Such a clear defect repair technique is indispensable in att- PSM fabrication.
PERSONAL Sign in with your SPIE account to access your personal subscriptions or to use specific features such as save to my library, sign up for alerts, save searches, etc.