24 March 2006 Tri-layer resist process for fabricating sub 45-nm L&S patterns by EPL
Author Affiliations +
Abstract
In this study, we have demonstrated a resist process to fabricate sub 45-nm lines and spaces (L&S) patterns (1:1) by using electron projection lithography (EPL) for a back-end-of-line (BEOL) process for 45-nm technology node. As a starting point we tried to fabricate sub 45-nm L&S (1:1) patterns using a conventional EPL single-layer resist process. There, the resolution of the EPL resist patterns turned out to be limited to 70 nm L&S (1:1) with aspect ratio (AR) of 3.3 which was caused by pattern collapse during the drying step in resist develop process. It has been common knowledge that pattern collapse of this type could be prevented by reducing the surface tension of the rinse-liquid and by decreasing the AR of the resist patterns. Therefore, we first applied a surfactant rinse to a single-layer resist process that could control the pattern collapse by its reduced surface tension. In this experiment, we used the ArF resist instead of the EPL resist because the surfactant that we were able to obtain was the one optimized to the ArF resist materials. From the results of ArF resist experiments, it was guessed that it was difficult for the EPL resist to obtain the L&S patterns with AR of 3.5 or more even if we used the surfactant optimized to the EPL resist. And we found that it was considerably difficult to form 45-nm L&S patterns with AR of 5.1 that was our target. Next, we evaluated a EPL tri-layer resist process to prevent pattern collapse by decreasing the AR of the resist patterns. Because in a tri-layer resist process the purpose of the top-layer resist is to transfer pattern to the middle-layer, a thinner top-layer resist was selected. By using the tri-layer resist process we were able to control the resist pattern collapse and thus were successful in achieving 40-nm L/S (1:1) top-layer resist patterns with AR of 2.3. The process also gave us 40-nm L&S (1:1) patterns after low-k film etching. And moreover, using our tri-layer resist process we were able to fabricate a wiring device with Cu/low-k. Although it was our first attempt, the process resulted in a high yield of 70 % for a 60-nm (1:1) wiring device. As a part of our study we conducted failure analysis of the results of our experiment. We found that the failures were located at the edge of the wafer and might originate in the bottom-layer pattern collapse. We thought that the wiring yield could be increased by control the bottom-layer pattern collapse. These findings indicated that our tri-layer resist process had a high applicability for device fabrication in BEOL.
© (2006) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Fumihiro Koba, Kazuyuki Matsumaro, Eiichi Soda, Tadayoshi Watanabe, Yoshihisa Matsubara, Hiroshi Arimoto, Tasuku Matsumiya, Daisuke Kawana, Naoki Yamashita, Yasushi Fujii, Katsumi Ohmori, Mitsuru Sato, Takahiro Kozawa, and Seiichi Tagawa "Tri-layer resist process for fabricating sub 45-nm L&S patterns by EPL", Proc. SPIE 6151, Emerging Lithographic Technologies X, 615127 (24 March 2006); https://doi.org/10.1117/12.655976
Lens.org Logo
CITATIONS
Cited by 5 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Photoresist processing

Failure analysis

Etching

Back end of line

Critical dimension metrology

Semiconducting wafers

Electron beam lithography

Back to Top