4 January 2008 The specimen preparation methods for nanoindentation testing of biomaterials: a review
Author Affiliations +
Abstract
Nanoindenter provides an approach for assessing mechanical properties in micro-electronics devices and films based on quantitative, controlled nanoindentation of surfaces, with the convenience of modern automation. It is also suitable to measure mechanical properties of biomaterials. Nanoindenter for biomaterial testing in bone and dentin was widely used. Recently some studies of nanoindentation properties in insect were carried out. While the surface roughness of natural biomaterials problem should not to be ignored in nanoindentation testing. The surface roughness will critically affect the precision of result of nanoindentation testing and caused error data. In this paper, the biomaterials specimen preparation methods for nanoindentation testing will be reviewed.
© (2008) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
J. Y. Sun, J. Tong, and Z. J. Zhang "The specimen preparation methods for nanoindentation testing of biomaterials: a review", Proc. SPIE 6831, Nanophotonics, Nanostructure, and Nanometrology II, 68310H (4 January 2008); https://doi.org/10.1117/12.756306
PROCEEDINGS
6 PAGES


SHARE
Advertisement
Advertisement
Back to Top