Prolonged exposure of chemical vapor deposited, polycrystalline ZnSe to high ac voltages in a 1 molal NaCl solution induces severe mechanical damage. Exposure produces defects that originate at the surface and grow intergranularly into the bulk with a bush-like morphology. Single crystal KRS-5 exposed to the same environmental conditions does not display the same mechanical damage. Possible causes for the degradation are discussed.
© (1991) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Joseph Allson King "Corrosion of ZnSe by alternating high voltage in a saline solution", Proc. SPIE 1535, Passive Materials for Optical Elements, (1 November 1991); https://doi.org/10.1117/12.48318
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Photomicroscopy

Crystals

Chemical vapor deposition

Corrosion

Optical components

Reflection

Chemical elements

Back to Top